检查模具和进料口:确保模具没有损坏或污染。检查进料口是否有毛刺或堵塞,清理干净后再试。

Check the Mold and Feed Port: Make sure the mold is not damaged or contaminated. Check the feed port for burrs or blockages, and clean it before trying again.

调整进料速度和温度:如果进料速度过快或温度过高,可能导致料流不均匀,从而在进料口形成痕迹。可以调整进料速度和温度,确保熔体流动平稳。

Adjust Feed Speed and Temperature: If the feed speed is too fast or the temperature is too high, it can cause uneven material flow, leaving marks at the feed port. Adjust the feed speed and temperature to ensure smooth material flow.

使用合适的原料:确保所用尼龙原料没有受到潮湿或污染,优质干燥的尼龙能减少进料口的痕迹。

Use Proper Materials: Ensure the nylon material used is not moist or contaminated. High-quality, dried nylon can reduce marks at the feed port.

优化生产工艺:根据产品要求调整注塑机的压力、温度和速度,确保更均匀的料流。

Optimize Production Process: Adjust the injection molding machine's pressure, temperature, and speed according to product requirements for a more even material flow.

定期维护设备:定期检查并清洁注塑机的进料系统,以确保其正常运作。

Regular Maintenance of Equipment: Regularly inspect and clean the injection molding machine's feeding system to ensure proper operation.